We are glad to share with you about the results of our work, company news, and give you timely developments and personnel appointment and removal conditions.
Bigely Technology's potassium chloride galvanizing brightener BZ-528 has a current efficiency of more than 98%. And the current density range is wide, which...
What precautions should we pay attention to during the passivation process of different workpieces when using trivalent chromium colored zinc passivation ag...
The nickel sulfamate plating process requires special attention to the following aspects during operation to ensure the quality of the plated layer and to s...
As we all know, in the production process of plastic plating, the colloidal palladium adsorbed on the surface of the plastic workpiece after palladium activ...
We all know that in the production process of plastic electroplating, the colloidal palladium adsorbed on the surface of plastic workpieces after palladium ...
Electroless copper plating is a process in which copper ions are reduced by reducing agent and deposited on the surface of conductive substrate without cur...
In the nickel plating process, white spots on the plated layer is a relatively common problem, which not only affects the aesthetics of the plated layer, bu...
We all know that in the production process of using nickel plating brighteners, blackening of the low area coating of workpieces is a common fault phenomeno...