Recently, a friend reported that during the production process using alkaline zinc nickel alloy additives, the workpiece will have blackening at the hook, which will seriously affect the appearance quality of the workpiece. So what causes the coating on the workpiece to turn black?

Bigely Technology has analyzed the characteristics of alkaline zinc nickel alloy additives based on on-site experience and products, mainly including the following four points:

1.Low zinc and high nickel in the plating solution can easily cause poor dispersion ability of the plating solution, resulting in blackening of the hooks on the workpiece. During the production process, the quality concentration of zinc and nickel in the plating solution should be controlled within the process range.

alkaline zinc nickel alloy additives

2.Insufficient concentration of zinc nickel alloy brightener in the plating solution can affect the co deposition of zinc nickel alloy and result in poor dispersion ability of the plating solution. During the production process, the concentration of the brightener can be determined and adjusted within the normal range using the Hull cell experiment.

3.The influence of metal impurities in the plating solution. As production progresses, the content of metal impurities in the plating solution will continue to accumulate. When the content of metal impurities is high, the dispersion ability of the plating solution is poor, and the coating will also have blackening phenomenon. During the production process, 0 # zinc plate should be used to reduce the dissolution of other metal impurities, and electrolytic treatment should be used regularly to treat the plating solution.

4.The concentration of sodium carbonate in the plating solution is relatively high. The high concentration of sodium carbonate can reduce the current efficiency of the cathode, affect the co deposition of zinc nickel alloy, and lead to blackening of the coating. The high content of sodium carbonate in the plating solution can be achieved by using freezing method to lower the bath temperature to around 5 ℃. Sodium carbonate will crystallize and precipitate, and filtering the plating solution can remove a large amount of sodium carbonate.

Therefore, the blackening phenomenon of zinc nickel alloy workpieces at the hook is often caused by poor dispersion ability of the plating solution. In the production process, pay more attention to the above four points to maintain better uniformity and dispersion ability of the plating solution, and also to better use alkaline zinc nickel alloy additives. If you are interested in alkaline zinc nickel alloy additives, please contact Bigely customer service for free samples and detailed technical information!