In the production process of using electroless nickel plating solution, it is important to control the deposition rate of the chemical nickel layer to ensure production efficiency and stability of the plating solution. So what are the factors that affect the deposition rate of coatings?
1.Nickel salt. Nickel salt is the main component of the plating solution. Generally, as the concentration of nickel salt increases, the deposition rate of the coating will accelerate. When the concentration of nickel salt is greater than 30g/L, the increase in sedimentation rate is not significant; When the concentration of nickel salt exceeds 40g/L, precipitates will appear in the plating solution.
2.Sodium hypophosphite. Sodium hypophosphite is a reducing agent in the plating solution. As the concentration of sodium hypophosphite increases, the deposition rate accelerates, but the stability of the plating solution deteriorates. When the concentration of sodium hypophosphite exceeds 30g/L, particles begin to appear in the plating solution.
3.Chelating agent. The function of complexing agents is to reduce the concentration of free Ni2+ in the plating solution and prevent the precipitation of nickel sulfite and nickel hydroxide. Generally, as the concentration of chelating agents increases, the sedimentation rate will decrease, but the magnitude is not significant.
4.Buffer agent. Buffer agents can prevent rapid changes in the pH value of the plating solution. When the buffer concentration is between 12-20g/L, the sedimentation rate remains relatively constant; When the concentration of buffer is greater than 24g/L, the sedimentation rate will significantly decrease.
5.Stabilizers. Stabilizers have a significant stabilizing effect on the plating solution, as they quickly reduce the deposition rate.
6.Temperature. Temperature is one of the important factors affecting the deposition rate of chemical nickel, and as the temperature increases, the deposition rate significantly accelerates. But the temperature of the plating solution should not be too high. When the temperature exceeds 95 ℃, the plating solution will lose control due to the fast deposition rate, triggering the self decomposition of the plating solution.
7.PH value. When the pH is greater than 3, the sedimentation rate will increase as the pH value increases. When the pH value is greater than 6, the deposition rate is faster, but the stability of the plating solution decreases. To obtain a bright coating, it is recommended to control the pH value between 4.5 and 5.5.
So, in the production process of using electroless nickel plating solution, we should pay attention to the above 7 factors that will affect the deposition rate of the coating. If you are interested in electroless nickel plating solution, please contact Bigely customer service for free samples and detailed technical information!