5 reasons why the coating on the workpiece is prone to positive and negative surfaces when using a new plating solution with acidic zinc plating brightener

2026-11-27 09:01:54

A friend left a message saying that when using a newly prepared plating solution with acidic zinc plating brightener, the workpiece coating is prone to the phenomenon of positive and negative surfaces, which affects the production quality. So what are the reasons for the appearance of positive and negative surfaces on the workpiece?

Bigely Technology has conducted an analysis based on on-site experience and the characteristics of the acidic zinc plating brightener product. The main reasons are as follows:

1.The concentration of brightener in the plating solution is too low or no brightener is added. Brightening agents can make the coating bright and level. When the concentration of the brightening agent is too low or no brightening agent is added, the coating will exhibit a phenomenon of positive and negative surfaces. During the production process, the concentration of brightener can be analyzed and adjusted through the Hull cell test.

acidic zinc plating brightener

2.The cathode current density is too low. During the electroplating process, the current density is low, the deposition rate of the coating is slow, and the phenomenon of positive and negative surfaces is prone to occur. Therefore, the cathode current density should be controlled within the process range according to production needs, for example, the current density of BZ-528 can be controlled within the range of 0.5~3.0A/dm2.

3.Excessive workpiece loading or insufficient anode area. During the electroplating process, the workpiece may have difficulty obtaining a normal coating due to the large coverage area, resulting in the appearance of positive and negative surfaces on the coating. In this situation, the loading capacity of the workpiece should be appropriately reduced or the anode area should be increased to obtain a uniform and bright coating on the workpiece.

4.Uneven inflation. Some acidic zinc plating brighteners require pumping and stirring during use in order to obtain a uniform coating on the workpiece. But when the plating solution is inflated, the hanging plated parts are prone to falling off the groove. If the inflation is uneven, the workpiece will exhibit a phenomenon of positive and negative surfaces. It is recommended to use Bigely's BZ-528 acid zinc plating brightener here. There is no need to inflate during the production process, and the workpiece can obtain a uniform and bright coating.

5.The design of the workpiece hanger is unreasonable. Due to the unreasonable design of hanging fixtures in some production lines, the workpieces are hung too tightly. During the production process, the workpieces are obstructed by each other, resulting in uneven distribution of power lines and the appearance of positive and negative surfaces on the workpieces.

Therefore, when using acidic zinc plating brightener, we should pay attention to the above 5 points, which can avoid the phenomenon of positive and negative surfaces on the workpiece, reduce the occurrence of faults, and improve production efficiency. If you are interested in acidic zinc plating brightener, please contact Bigely customer service for free samples and detailed technical information!